I was told that I could use lime, sand or vermiculite...I had vermiculite.
Maybe I don't understand, but aren't they all insulators? I thought that was the purpose. You spend an hour or so bringing the insulating material up to temperature, then you bury the part in it, and it insulates the part against temperature spikes, allowing it to bath in uniform heat to temper.
Did I mis-understand the process?
the frizzen...or hammer, if you will...is sparking better, but if it doesn't do well enough with more use, I'll re-do it using either sand or lime.