Case hardening or pack hardening, is quenched at red heat. The molecular skin of higher content carbon steel should be file hard. Any heating thereafter, to straw, for example, at 375 deg F or to shiny blue at 550 - 700 degrees, will make the surface softer, or as Hugh says, will anneal the surface. That is the way that I understand it, anyway.