« Reply #25 on: October 07, 2008, 05:17:32 PM »
A bit to the side of the topic, but when I boil rust blued parts I use hard water form a local artesian well and the mineral built up on the boiled part and do a better blue (in terms on tone, evenness) than distilled water. It is of interest "lime" it stops heat blue...