Author Topic: Soled frizzen  (Read 974 times)

Offline rich pierce

  • Administrator
  • Hero Member
  • *
  • Posts: 19632
Soled frizzen
« on: June 14, 2018, 06:50:00 PM »
Here is an original soled frizzen. Interesting to see thickness of the sole. Perhaps never tempered after riveting. Not sure why else it would break like that.



Andover, Vermont

Offline stubshaft

  • Sr. Member
  • ****
  • Posts: 368
Re: Soled frizzen
« Reply #1 on: June 14, 2018, 08:07:47 PM »
Could've had a fracture from the square cut rivet.
I'd rather die standing, than live on my knees...

Offline deepcreekdale

  • Hero Member
  • *****
  • Posts: 641
Re: Soled frizzen
« Reply #2 on: June 14, 2018, 11:22:41 PM »
Very interesting picture. Just an aside, while doing research on Spanish weapons I found they often made their soles so they could be screwed on to the frizzen. When worn out, they just made another one, tapped it, hardened and screwed it back on. Pretty practical solution.
”Far and away the best prize that life has to offer is the chance to work hard at work worth doing.” Theodore Roosevelt

Offline Bob Roller

  • Hero Member
  • *****
  • Posts: 9737
Re: Soled frizzen
« Reply #3 on: June 14, 2018, 11:38:32 PM »
Hard to the point of being brittle and the square rivet may well have contributed to its demise.
I recall seeing an article about frizzens faced with very hard "soles" fastened with screws on English military
locks that would be used in very cold climates like one of the poles.I think it's a good idea IF the job can
be done in a way that looks neat and not some kind of an expedient.

Bob Roller