Thanks to all for putting me on to the LMF browning. I really like how simole it is to use, and the good coverage results.
BUT, maybe now a problem.
After I was satisfied that everything is well browned, I took all the parts and carded with 0000 steel wool and scotchbrite. Still looked great.
Then I crubbed every part, WELL, with a slurry of baking soda and water, and used a stiff toothbrush like parts cleaning brush. All over and very well.
Then rinsed with HOT water from my 100ft+ garden hose laying in the sun.
Then I dried it all and let it set in the hot sun till bone dry, and it was even hot to the touch from the sun.
Then I wiped it all down generous amount of WD40. Then I used full stnthetic motor oil.
Finally paste wax and assembly.
Since then a coat or two of beeswax polish.
Looks great, but today I picked it up and my hands are covered in red rust!
Do I just need more oil or should I maybe take it all apart and rescrub with soda?
Man that makes alot more work?